Jianqiang Zhang

Professor

ABOUT ME

I am a professor in the School of Materials Science and Engineering at UNSW where I am doing both research and teaching. My research is focused on complex gas-solid reactions at high temperatures in application to steel/alloy high temperature corrosion and metallurgical technologies. I started the gas-solid reaction research when I carried out my PhD work in the field of process metallurgy on iron ore reduction and cementation. My high temperature corrosion research commenced at Max-Planck-Institute for Iron Research (MPIE) in Germany as a research scientist after my PhD. Three years research at MPIE in the field of high temperature corrosion laid a sound foundation for my further work at UNSW in this research area. I returned to UNSW in 2003, working in the high temperature group at the School of Materials Science and Engineering, first as a research associate and research fellow (2003-2005), Australian Research Fellow (2006-2010), a senior research fellow (2009-2011), a senior lecturer (2012- 2015), an associate professor (2015-2019), and a professor (2019-), and is now leading a research team in high temperature corrosion research.

PROFESSIONAL EXPERIENCE

  • Professor, School of Materials Science & Engineering, UNSW 2019
  • Associate Professor, School of Materials Science & Engineering, UNSW, 2015 - 2019
  • Senior Lecturer, School of Materials Science & Engineering, UNSW, 2012-2015
  • Senior Research Fellow, School of Materials Science & Engineering, UNSW, 2009-2011
  • Research Fellow, Research Associate, School of Materials Science & Engineering, UNSW, 2003-2009
  • Research Fellow, Max-Planck Institute for Iron Research, Germany, 2000-2003
  • Visiting Research Fellow, University of Newcaste, 1996
  • Associate Professor, Lecturer, Southeast University, China, 1987-1996

RESEARCH

High-temperature corrosion is essential for some important industries, such as electric power generating plants, aerospace, heat-treating, and mineral and metallurgical processing operated at high temperatures. The formation of corrosion products leads to the loss of materials, reduces reliability and stability, and finally decreases the service lifetime of the engineering components. It is therefore important to develop high temperature corrosion resistant materials.

Research goals

My research is focused on the understanding of the alloy-gas reactions in corrosion processes, the prediction of reaction products and kinetics as a function of temperature and the compositions of both alloy and gas, and finally the development of corrosion resistant high temperature alloys for high temperature application.

Research Contributions

Most significant contributions of my work are in the field of gas-solid reactions at high temperature, including high temperature corrosion and processing metallurgy. Research emphases are on the reaction thermodynamics and kinetics, phase transformation and characterisation, reaction mechanism understanding, sustainable materials processing, and new materials development. 

Major Research Projects

Journal articles
add
Xie Y; Cai Y; Zhang J; Gleeson B; Young DJ, 2021, 'Effects of Sulphate Deposits on Corrosion Behaviour of Fe-Based Alloys in Wet CO2 Gas at 750 °C', Oxidation of Metals, vol. 95, pp. 23 - 43, http://dx.doi.org/10.1007/s11085-020-10010-x
2021
Aye KK; Nguyen TD; Zhang J; Young DJ, 2021, 'Effect of silicon on corrosion of Fe-20Cr and Fe-20Cr-20Ni alloys in wet CO2 with and without HCl at 650 °C', Corrosion Science, vol. 179, http://dx.doi.org/10.1016/j.corsci.2020.109096
2021
Xie Y; Cai Y; Zhang J; Gleeson B; Young DJ, 2021, 'Effects of sulphate deposits on corrosion behaviour of Ni-base alloys in wet CO2 gas at 750 °C', Corrosion Science, vol. 181, http://dx.doi.org/10.1016/j.corsci.2020.109227
2021
Wang Q; Yang J; Zhang J; Ostrovski O; Zhang C; Cai D, 2021, 'Effect of Na2O on Properties, Structure, and Crystallization of CaO–Al2O3-Based Mold Fluxes', Steel Research International, http://dx.doi.org/10.1002/srin.202100193
2021
Yang J; Wang L; Wang Q; Zhang J; Sasaki Y; Zhang C; Cai D; Ostrovski O, 2021, 'Challenges in the Mold Flux Design: Development of F-Free Fluxes and Fluxes for Casting of High-Al Steel', Steel Research International, pp. 2100123 - 2100123, http://dx.doi.org/10.1002/srin.202100123
2021
Zhang JQ, 2021, 'Co2 high temperature corrosion and its prevention of chromia forming fe-base alloys', Surface Technology, vol. 50, pp. 260 - 266, http://dx.doi.org/10.16490/j.cnki.issn.1001-3660.2021.04.026
2021
Li M; Xie Y; Grzesik Z; Liu F; Zhang J; Zhou C, 2020, 'Effect of Ni-Al coating with and without re modification on coking and metal dusting of Fe-Cr-Ni alloy under cyclic condition at 600°C', Journal of the Electrochemical Society, vol. 167, http://dx.doi.org/10.1149/1945-7111/abd56d
2020
Jiang C; Li S; Liu H; Bao Z; Zhang J; Zhu S; Wang F, 2020, 'Effect of Hf addition in (Ni,Pt)Al bond coat on thermal cycling behavior of a thermal barrier coating system at 1100 °C', Corrosion Science, vol. 166, http://dx.doi.org/10.1016/j.corsci.2019.108424
2020
Nguyen TD; Zhang J; Young DJ, 2020, 'Effects of Si, Al and Ti on corrosion of Ni-20Cr and Ni-30Cr alloys in Ar-20CO2-20H2O gas at 700 °C', Corrosion Science, vol. 170, http://dx.doi.org/10.1016/j.corsci.2020.108702
2020
Jiang C; Xie Y; Kong C; Zhang J; Young DJ, 2020, 'Corrosion behaviour of Ni-Cr alloys in mixed oxidising gases at 650 °C', Corrosion Science, vol. 174, http://dx.doi.org/10.1016/j.corsci.2020.108801
2020
Xie Y; Zhang J; Young DJ, 2020, 'Effects of Fe on Oxidation of Ni-20Cr and Ni-30Cr Alloys at 800 °C in Wet CO2 Gas', Oxidation of Metals, vol. 94, pp. 219 - 233, http://dx.doi.org/10.1007/s11085-020-09987-2
2020
Aye KK; Zhang J; Young DJ, 2020, 'Effect of Hydrogen Chloride on Corrosion Behaviour of Fe–Cr Alloys in Wet CO2 Gas at 650 °C', Oxidation of Metals, vol. 94, pp. 51 - 80, http://dx.doi.org/10.1007/s11085-020-09978-3
2020
Xi X; Kong C; Zhang J, 2020, 'Effect of Cyclic Reaction on Corrosion Behavior of Chromium-Containing Alloys in CO2 Gas at 650 °C', Oxidation of Metals, vol. 93, pp. 131 - 157, http://dx.doi.org/10.1007/s11085-019-09950-w
2020
Solimani A; Nguyen T; Zhang J; Young DJ; Schütze M; Galetz MC, 2020, 'Morphology of oxide scales formed on chromium-silicon alloys at high temperatures', Corrosion Science, vol. 176, http://dx.doi.org/10.1016/j.corsci.2020.109023
2020
Xie Y; Liang T; Zhang J; Young DJ, 2020, 'Effects of Fe on oxidation of Ni-20Cr and Ni-30Cr alloys at 800 °C in dry CO2 gas', Corrosion Science, vol. 173, http://dx.doi.org/10.1016/j.corsci.2020.108777
2020
Yang J; Zhang J; Ostrovski O; Sasaki Y; Zhang C; Cai D, 2019, 'Dynamic Wetting of High-Al Steel by CaO-SiO2- and CaO-Al2O3-Based Mold Fluxes', Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, vol. 50, pp. 2175 - 2185, http://dx.doi.org/10.1007/s11663-019-01643-8
2019
Yang J; Wang Q; Zhang J; Ostrovski O; Zhang C; Cai D, 2019, 'Effect of Al2O3/(B2O3+ Na2O) Ratio on CaO-Al2O3-Based Mold Fluxes: Melting Property, Viscosity, Heat Transfer, and Structure', Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, vol. 50, pp. 2794 - 2803, http://dx.doi.org/10.1007/s11663-019-01711-z
2019
Yang J; Cui H; Zhang J; Ostrovski O; Zhang C; Cai D, 2019, 'Interfacial Reaction Between High-Al Steel and CaO-Al2O3-Based Mold Fluxes with Different CaO/Al2O3 Ratios at 1773 K (1500 °C)', Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, vol. 50, pp. 2636 - 2646, http://dx.doi.org/10.1007/s11663-019-01667-0
2019
Yu CT; Liu H; Zhang J; Ullah A; Bao ZB; Jiang CY; Zhu SL; Wang FH, 2019, 'Gradient thermal cycling behavior of a thermal barrier coating system constituted by NiCoCrAlY bond coat and pure metastable tetragonal nano-4YSZ top coat', Ceramics International, vol. 45, pp. 15281 - 15289, http://dx.doi.org/10.1016/j.ceramint.2019.05.018
2019
Li M; Kong C; Zhang J; Zhou C; Young DJ, 2019, 'Oxidation behavior of Ni-Al coating with and without a Ni-Re diffusion barrier in dry CO 2 gas at 650 ºC', Corrosion Science, vol. 149, pp. 236 - 243, http://dx.doi.org/10.1016/j.corsci.2019.01.021
2019
Yuan X; Wang L; Zhang J; Ostrovski O; Zhang C; Cai D, 2019, 'Modelling of viscosity of fluorine-free mold fluxes using neural network', Metallurgical Research and Technology, vol. 116, http://dx.doi.org/10.1051/metal/2018053
2019
Yang J; Zhang J; Ostrovski O; Zhang C; Cai D, 2019, 'Flux-steel reaction of CaO-SiO2 and CaO-Al2O3-based mold fluxes with high-Al steel', Metallurgia Italiana, vol. 111, pp. 12 - 19
2019
Yang J; Cui H; Zhang J; Ostrovski O; Zhang C; Cai D, 2019, 'Effect of Na2O on the Interfacial Reaction between CaO–Al2O3 based Mold Fluxes and High-Al Steel at 1 500°C', ISIJ International, vol. 59, pp. 2247 - 2255, http://dx.doi.org/10.2355/isijinternational.ISIJINT-2019-257
2019
Wu H; Jiang C; Zhang J; Huang S; Wang L; Jiao S; Huang H; Jiang Z, 2019, 'Oxidation Behaviour of Steel During hot Rolling by Using TiO2-Containing Water-Based Nanolubricant', Oxidation of Metals, vol. 92, pp. 315 - 335, http://dx.doi.org/10.1007/s11085-019-09924-y
2019
Wu Q; Xu Y; Zhang J; Zhong N; Fan C; Chang X; Zhang X, 2019, 'Corrosion behaviour of TiC particle-reinforced 304 stainless steel in simulated marine environment at 650°C', ISIJ International, vol. 59, pp. 336 - 344, http://dx.doi.org/10.2355/isijinternational.ISIJINT-2018-534
2019
Yang J; Zhang J; Ostrovski O; Zhang C; Cai D, 2019, 'Effects of B2O3 on Crystallization, Structure, and Heat Transfer of CaO-Al2O3-Based Mold Fluxes', Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, vol. 50, pp. 291 - 303, http://dx.doi.org/10.1007/s11663-018-1467-5
2019
Chen C; Liu N; Zhang J; Cao J; Wang LJ; Xiang HF, 2019, 'Microstructure stability and oxidation behaviour of (FeCoNiMo)90(Al/Cr)10 high-entropy alloys', Materials Science and Technology (United Kingdom), vol. 35, pp. 1883 - 1890, http://dx.doi.org/10.1080/02670836.2019.1652785
2019
Wang Q; Yang JA; Zhang C; Cai DX; Zhang JQ; Ostrovski O, 2019, 'Effect of CaO/Al2O3 ratio on viscosity and structure of CaO–Al2O3-based fluoride-free mould fluxes', Journal of Iron and Steel Research International, vol. 26, pp. 374 - 384, http://dx.doi.org/10.1007/s42243-019-00248-4
2019
Yang J; Zhang J; Ostrovski O; Zhang C; Cai D, 2019, 'Effects of Fluorine on Solidification, Viscosity, Structure, and Heat Transfer of CaO-Al2O3-Based Mold Fluxes', Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, vol. 50, pp. 1766 - 1772, http://dx.doi.org/10.1007/s11663-019-01579-z
2019
Nguyen TD; Zhang J; Young DJ, 2018, 'Effects of Si, Al and Ti on corrosion of Ni-20Cr and Ni-30Cr alloys in Ar-20CO2 at 700 °C', Corrosion Science, vol. 130, pp. 161 - 176, http://dx.doi.org/10.1016/j.corsci.2017.11.005
2018
Li M; Li N; Zhang J; Zhou C, 2018, 'Inhibiting effect of Ni-Re interlayer between Ni-Al coating and steel substrate on interdiffusion and carburization', Surface and Coatings Technology, vol. 337, pp. 68 - 74, http://dx.doi.org/10.1016/j.surfcoat.2017.12.065
2018
Xie Y; Nguyen TD; Zhang J; Young DJ, 2018, 'Corrosion behaviour of Ni-Cr alloys in wet CO2 atmosphere at 700 and 800 °C', Corrosion Science, vol. 146, pp. 28 - 43, http://dx.doi.org/10.1016/j.corsci.2018.10.029
2018
Nguyen TD; La Fontaine A; Cairney JM; Zhang J; Young DJ, 2018, 'Effects of Si, Mn, and water vapour on the microstructure of protective scales grown on Fe–20Cr in CO2 gas', Materials at High Temperatures, vol. 35, pp. 22 - 29, http://dx.doi.org/10.1080/09603409.2017.1389098
2018
Jullian D; Zhang J; Hibbert DB; Young DJ, 2018, 'Oxygen solubility in austenitic Fe-Ni alloys at high temperatures', Journal of Alloys and Compounds, vol. 732, pp. 646 - 654, http://dx.doi.org/10.1016/j.jallcom.2017.10.226
2018
Nguyen TD; Zhang J; Young DJ, 2018, 'Growth of Cr2O3 blades during alloy scaling in wet CO2 gas', Corrosion Science, vol. 133, pp. 432 - 442, http://dx.doi.org/10.1016/j.corsci.2018.01.045
2018
Zhang J, 2018, 'High temperature corrosion research at unsw', Corrosion and Materials, vol. 43, pp. 42 - 43
2018
Nguyen TD; La Fontaine A; Yang L; Cairney JM; Zhang J; Young DJ, 2018, 'Atom probe study of impurity segregation at grain boundaries in chromia scales grown in CO2 gas', Corrosion Science, vol. 132, pp. 125 - 135, http://dx.doi.org/10.1016/j.corsci.2017.12.024
2018
Zhang J; Garcia-Fresnillo L; Jalowicka A; Pillai R; Naumenko D; Quadakkers WJ, 2018, 'Phase Transformations in Co-Ni-Cr-W Alloys During High Temperature Exposure to Steam Environment', Journal of Phase Equilibria and Diffusion, vol. 39, pp. 387 - 400, http://dx.doi.org/10.1007/s11669-018-0647-y
2018
Young DJ; Zhang J, 2018, 'Alloy Corrosion by Hot CO2 Gases', JOM, vol. 70, pp. 1493 - 1501, http://dx.doi.org/10.1007/s11837-018-2944-7
2018
Yang J; Zhang J; Sasaki Y; Ostrovski O; Zhang C; Cai D; Kashiwaya Y, 2018, 'Effect of MgO on Crystallization and Heat Transfer of Fluoride-Free Mold Fluxes', Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, vol. 49, pp. 3097 - 3106, http://dx.doi.org/10.1007/s11663-018-1380-y
2018
Wu Q; Zhang J, 2018, 'Corrosion behavior of laser-clad Cu-9Ni-6Sn coating', Surface and Coatings Technology, vol. 349, pp. 1117 - 1129, http://dx.doi.org/10.1016/j.surfcoat.2018.07.012
2018
Xie Y; Zhang J; Young DJ, 2018, 'Water vapour effects on corrosion of Ni-Cr alloys in CO2 gas at 650 °C', Corrosion Science, vol. 136, pp. 311 - 325, http://dx.doi.org/10.1016/j.corsci.2018.03.023
2018
McCarroll IE; La Fontaine A; Nguyen TD; Smith AF; Zhang J; Young DJ; Cairney JM, 2018, 'Performance of an FeCrAl alloy in a high-temperature CO2 environment', Corrosion Science, vol. 139, pp. 267 - 274, http://dx.doi.org/10.1016/j.corsci.2018.05.007
2018
Wang L; Zhang C; Cai D; Zhang J; Sasaki Y; Ostrovski O, 2017, 'Effects of CaO/SiO2 Ratio and Na2O Content on Melting Properties and Viscosity of SiO2-CaO-Al2O3-B2O3-Na2O Mold Fluxes', Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, vol. 48, pp. 516 - 526, http://dx.doi.org/10.1007/s11663-016-0816-5
2017
Nguyen TD; Xie Y; Ding S; Zhang J; Young DJ, 2017, 'Oxidation Behavior of Ni–Cr Alloys in CO2 at 700 °C', Oxidation of Metals, vol. 87, pp. 605 - 616, http://dx.doi.org/10.1007/s11085-017-9721-9
2017
Jullian D; Prillieux A; Zhang J; Young DJ, 2017, 'Oxygen permeability of Fe-Ni-Cr alloys at 1100 and 1150 °C under carbon-free and carbon-containing gases', Materials and Corrosion, vol. 68, pp. 197 - 204, http://dx.doi.org/10.1002/maco.201508803
2017
Wang L; Zhang J; Sasaki Y; Ostrovski O; Zhang C; Cai D, 2017, 'Stability of Fluorine-Free CaO-SiO2-Al2O3-B2O3-Na2O Mold Fluxes', Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, vol. 48, pp. 1055 - 1063, http://dx.doi.org/10.1007/s11663-016-0907-3
2017
Yu C; Zhang J; Young DJ, 2017, 'Corrosion Behaviour of Fe–Cr–(Mn, Si) Ferritic Alloys in Wet and Dry CO2–SO2Atmospheres at 650 °C', Oxidation of Metals, vol. 90, pp. 1 - 22, http://dx.doi.org/10.1007/s11085-017-9826-1
2017
Nguyen TD; Zhang J; Young DJ, 2017, 'Effects of Silicon and Water Vapour on Corrosion of Fe–20Cr and Fe–20Cr–20Ni Alloys in CO2 at 650 °C', Oxidation of Metals, vol. 87, pp. 541 - 573, http://dx.doi.org/10.1007/s11085-016-9681-5
2017
Kapelyushin Y; Sasaki Y; Zhang J; Jeong S; Ostrovski O, 2017, 'Formation of a Network Structure in the Gaseous Reduction of Magnetite Doped with Alumina', Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, vol. 48, pp. 889 - 899, http://dx.doi.org/10.1007/s11663-016-0897-1
2017
Nguyen TD; Peng X; Zhang J; Young DJ, 2017, 'Corrosion resistance of chromised and aluminised coatings in wet CO2 gas at 650 °C', Surface and Coatings Technology, vol. 316, pp. 226 - 238, http://dx.doi.org/10.1016/j.surfcoat.2017.03.028
2017
Xie Y; Zhang J; Young DJ, 2017, 'Temperature Effect on Oxidation Behaviour of Ni-Cr Alloys in CO2 Gas Atmosphere', Journal of the Electrochemical Society, vol. 164, pp. C285 - C293, http://dx.doi.org/10.1149/2.1021706jes
2017
Prillieux A; Jullian D; Zhang J; Monceau D; Young DJ, 2017, 'Internal Oxidation in Dry and Wet Conditions for Oxygen Permeability of Fe–Ni Alloys at 1150 and 1100 °C', Oxidation of Metals, vol. 87, pp. 273 - 283, http://dx.doi.org/10.1007/s11085-017-9724-6
2017
Xie Y; Zhang J; Young DJ, 2017, 'Effect of temperature on oxidation behavior of Ni-Cr alloys in CO2', ECS Transactions, vol. 68, pp. 171 - 185
2017
Yu C; Zhang J; Young DJ, 2016, 'High temperature corrosion of Fe-Cr-(Mn/Si) alloys in CO2-H2O-SO2 gases', Corrosion Science, vol. 112, pp. 214 - 225, http://dx.doi.org/10.1016/j.corsci.2016.07.026
2016
Nguyen TD; Zhang J; Young DJ, 2016, 'Effect of Mn on oxide formation by Fe-Cr and Fe-Cr-Ni alloys in dry and wet CO2 gases at 650 °C', Corrosion Science, vol. 112, pp. 110 - 127, http://dx.doi.org/10.1016/j.corsci.2016.07.014
2016
Yu C; Nguyen TD; Zhang J; Young DJ, 2016, 'Sulfur Effect on Corrosion Behavior of Fe-20Cr-(Mn, Si) and Fe-20Ni-20Cr-(Mn, Si) in CO2-H2O at 650°C', Journal of the Electrochemical Society, vol. 163, pp. C106 - C115, http://dx.doi.org/10.1149/2.0751603jes
2016
Kapelyushin Y; Sasaki Y; Zhang J; Jeong S; Ostrovski O, 2016, 'Effects of Temperature and Gas Composition on Reduction and Swelling of Magnetite Concentrates', Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, vol. 47, pp. 2263 - 2278, http://dx.doi.org/10.1007/s11663-016-0719-5
2016
Zhang Y; Guo P; Shao Y; Lai Y; Zhang J, 2016, 'Preparation and high-temperature performance of Co-10Mn and Co-40Mn alloy coatings for solid oxide fuel cell metal interconnects', Journal of Alloys and Compounds, vol. 680, pp. 685 - 693, http://dx.doi.org/10.1016/j.jallcom.2016.04.183
2016
Zhang C; Min X; Zhang J; Wang M; Li Y; Fei J, 2016, 'Reductive clean leaching process of cadmium from hydrometallurgical zinc neutral leaching residue using sulfur dioxide', Journal of Cleaner Production, vol. 113, pp. 910 - 918, http://dx.doi.org/10.1016/j.jclepro.2015.11.059
2016
Zhang C; Min XB; Zhang JQ; Wang M; Li YC, 2016, 'Mechanisms and kinetics on reductive leaching of zinc from zinc neutral leaching residue', Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, vol. 26, pp. 197 - 203
2016
La Fontaine A; Gault B; Breen A; Stephenson L; Ceguerra AV; Yang L; Dinh Nguyen T; Zhang J; Young DJ; Cairney JM, 2015, 'Interpreting atom probe data from chromium oxide scales', Ultramicroscopy, vol. 159, pp. 354 - 359, http://dx.doi.org/10.1016/j.ultramic.2015.02.005
2015
Nguyen TD; Zhang JQ; Young DJ, 2015, 'Microstructures of chromia scales grown in CO 2', Materials at High Temperatures, vol. 32, pp. 16 - 21, http://dx.doi.org/10.1179/0960340914Z.00000000056
2015
Nguyen TD; Zhang J; Young DJ, 2015, 'Effects of cerium and manganese on corrosion of Fe-Cr and Fe-Cr-Ni alloys in Ar-20CO2 and Ar-20CO2-20H2O gases at 650°C', Corrosion Science, vol. 100, pp. 448 - 465, http://dx.doi.org/10.1016/j.corsci.2015.08.012
2015
Kapelyushin Y; Xing X; Zhang J; Jeong S; Sasaki Y; Ostrovski O, 2015, 'Effect of Alumina on the Gaseous Reduction of Magnetite in CO/CO2 Gas Mixtures', Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, vol. 46, pp. 1175 - 1185, http://dx.doi.org/10.1007/s11663-015-0316-z
2015
Zhang C; Min X; Chai L; Zhang J; Wang M, 2015, 'Mechanical Activation-Assisted Reductive Leaching of Cadmium from Zinc Neutral Leaching Residue Using Sulfur Dioxide', JOM, vol. 67, pp. 3010 - 3021, http://dx.doi.org/10.1007/s11837-015-1623-1
2015
Kapelyushin Y; Sasaki Y; Zhang J; Jeong S; Ostrovski O, 2015, 'In-Situ Study of Gaseous Reduction of Magnetite Doped with Alumina Using High-Temperature XRD Analysis', Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, vol. 46, pp. 2564 - 2572, http://dx.doi.org/10.1007/s11663-015-0437-4
2015
Zhang C; Min X; Zhang J; Wang M; Fei J; Li Y, 2015, 'Enhanced Cadmium Extraction from Zinc Neutral Leaching Residue Using Sulfur Dioxide', Separation Science and Technology (Philadelphia), vol. 50, pp. 2688 - 2696, http://dx.doi.org/10.1080/01496395.2015.1078356
2015
Zhang C; Min XB; Zhang JQ; Wang M; Zhou BS; Shen C, 2015, 'Reductive acid leaching of cadmium from zinc neutral leaching residue using hydrazine sulfate', Transactions of Nonferrous Metals Society of China (English Edition), vol. 25, pp. 4175 - 4182, http://dx.doi.org/10.1016/S1003-6326(15)64068-7
2015
Zhang C; Min XB; Wang M; Zhang JQ; Li YC, 2015, 'Mechanochemical stabilizing behavior of lead in the lead-containing smelting slag', Guocheng Gongcheng Xuebao/The Chinese Journal of Process Engineering, vol. 15, pp. 1035 - 1038
2015
Zhang C; Zhang J; Min X; Wang M; Zhou B; Shen C, 2015, 'Kinetics of Reductive Acid Leaching of Cadmium-Bearing Zinc Ferrite Mixture Using Hydrazine Sulfate', JOM, vol. 67, pp. 2028 - 2037, http://dx.doi.org/10.1007/s11837-015-1553-y
2015
Nguyen T; Zhang J; Young D, 2015, 'Effect of Si on corrosion of Fe-Cr and Fe-Ni-Cr alloys in wet CO2 gas', Corrosion Science and Technology, vol. 32, pp. 16 - 21, http://dx.doi.org/10.14773/cst.2015.14.3.127
2015
Yu C; Nguyen TD; Zhang J; Young D, 2015, 'Effect of Sulphur on Fe-20Cr-(Mn, Si) Alloy Corrosion in CO2-H2O Gases at 650°C', ECS Transactions, vol. 66, pp. 23 - 39
2015
Nguyen TD; Zhang J; Young DJ, 2015, 'Water Vapor Effects on Corrosion of Fe–Cr and Fe–Cr–Ni Alloys Containing Silicon in CO2 Gas at 818 °C', Oxidation of Metals, http://dx.doi.org/10.1007/s11085-015-9536-5
2015
Nguyen TD; Zhang J; Young DJ, 2015, 'Effects of cerium and manganese on corrosion of Fe-Cr and Fe-Cr-Ni alloys in Ar-20CO2 and Ar-20CO2-20H2O gases at 650°C', Corrosion Science, http://dx.doi.org/10.1016/j.corsci.2015.08.012
2015
Nguyen TD; Zhang J; Young DJ, 2015, 'Water Vapor Effects on Corrosion of Fe–Cr and Fe–Cr–Ni Alloys Containing Silicon in CO2 Gas at 818 °C', Oxidation of Metals, vol. 83, pp. 575 - 594, http://dx.doi.org/10.1007/s11085-015-9536-5
2015
Yu C; Nguyen TD; Zhang J; Young DJ, 2015, 'Corrosion of Fe-9Cr-(Mn, Si) alloys in CO2-H2O-SO2 gases', Corrosion Science, vol. 98, pp. 516 - 529, http://dx.doi.org/10.1016/j.corsci.2015.05.040
2015
Nguyen TD; Zhang J; Young DJ, 2014, 'Water vapour effects on corrosion of Fe–Cr and Fe–Cr–Ni alloys containing cerium and manganese in CO2 gas at 818°C', Corrosion Science, vol. 89, pp. 220 - 235, http://dx.doi.org/10.1016/j.corsci.2014.08.029
2014
Young DJ; Nguyen TD; Felfer P; Zhang J; Cairney JM, 2014, 'Penetration of protective chromia scales by carbon', Scripta Materialia, vol. 77, pp. 29 - 32, http://dx.doi.org/10.1016/j.scriptamat.2014.01.009
2014
Guo P; Zhang J; Konrad CH; Young DJ, 2014, 'Oxygen permeability measurements in Ni using H2/H2O, CO/CO2 and Ni/NiO Rhines pack atmospheres', Oxidation of Metals: an international journal of the science of gas-solid reactions, vol. 83, pp. 223 - 235, http://dx.doi.org/10.1007/s11085-014-9511-6
2014
Zhu L; Zhu S; Wang F; Zhang J, 2014, 'Comparison of the cyclic oxidation behavior of a low expansion Ni+CrAlYSiN nanocomposite and a NiCrAlYSi coating', Corrosion Science, vol. 80, pp. 393 - 401, http://dx.doi.org/10.1016/j.corsci.2013.11.052
2014
Zhu L; Zhu S; Wang F; Zhang J, 2014, 'Comparison of the cyclic oxidation behavior of a low expansion Ni+CrAlYSiN nanocomposite and a NiCrAlYSi coating', Corrosion Science, vol. 80, pp. 393 - 401, http://dx.doi.org/10.1016/j.corsci.2013.11.052
2014
Nguyen TD; Zhang J; Young DJ, 2014, 'Effects of Silicon on High Temperature Corrosion of Fe–Cr and Fe–Cr–Ni Alloys in Carbon Dioxide', Oxidation of Metals, vol. 81, pp. 549 - 574, http://dx.doi.org/10.1007/s11085-013-9467-y
2014
Xiang Z; Zhang J; Kong C; Peng X, 2014, 'Effect of Pre-oxidation on Carburisation and Metal Dusting of Nano-crystalline Ni–Cr Alloys', Oxidation of Metals, vol. 81, pp. 645 - 660, http://dx.doi.org/10.1007/s11085-014-9472-9
2014
Slabbert G; Mulaudzi F; Cornish L; Papo J; Morudu V; Zhang J, 2013, 'The effect of the matrix structure on the metal dusting rate in hydrocarbon environments', Journal of the Southern African Institute of Mining and Metallurgy, vol. 113, pp. 81 - 90, http://dx.doi.org/
2013
Nguyen T; Zhang J; Young D, 2013, 'The effect of Cerium and Manganese on reaction of Fe-Cr and Fe-Cr-Ni alloys in Ar-20CO2 gas at 818 oC', Corrosion Science, vol. 76, pp. 231 - 242, http://dx.doi.org/10.1016/j.corsci.2013.06.046
2013
Nguyen TD; Zhang J; Young DJ, 2013, 'Effects of cerium and manganese on corrosion of Fe-Cr and Fe-Cr-Ni alloys in Ar-20CO gas at 818 °C', Corrosion Science, http://dx.doi.org/10.1016/j.corsci.2013.06.046
2013
Young DJ; Zhang J, 2012, 'Metal dusting: Catastrophic corrosion by carbon', JOM, vol. 64, pp. 1461 - 1469, http://dx.doi.org/10.1007/s11837-012-0476-0
2012
Naess MK; Young DJ; Zhang J; Olsen JE; Tranell G, 2012, 'Active oxidation of liquid silicon: Experimental investigation of kinetics', Oxidation of Metals, vol. 78, pp. 363 - 376, http://dx.doi.org/10.1007/s11085-012-9312-8
2012
Zhang J; Speck P; Young DJ, 2012, 'Metal Dusting of Alumina-Forming Creep-Resistant Austenitic Stainless Steels', Oxidation of Metals, vol. 77, pp. 167 - 187, http://dx.doi.org/10.1007/s11085-011-9279-x
2012
Zhang J; Young DJ, 2012, 'Contributions of Carbon Permeation and Graphite Nucleation to the Austenite Dusting Reaction: A Study of Model Fe-Ni-Cu Alloys', Corrosion Science, vol. 56, pp. 184 - 193, http://dx.doi.org/10.1016/j.corsci.2011.12.006
2012
Li H; Zhang J; Young DJ, 2012, 'Oxidation of Fe-Si, Fe-Al and Fe-Si-Al alloys in CO2-H2O gas at 800°C', Corrosion Science, vol. 54, pp. 127 - 138, http://dx.doi.org/10.1016/j.corsci.2011.09.006
2012
Gheno T; Zhang J; Young DJ, 2011, 'High temperature corrosion of chromia-forming alloys under oxyfuel firing conditions', 18th International Corrosion Congress 2011, vol. 2, pp. 1000 - 1008
2011
Wu Q; Zhang J; Young DJ, 2011, 'Metal dusting behaviour of several nickel- and cobalt-base alloys in CO-H2-H2O atmosphere', Materials and Corrosion - Werkstoffe und Korrosion, vol. 62, pp. 521 - 530, http://dx.doi.org/10.1002/maco.201005863
2011
Othman NK; Zhang J; Young DJ, 2011, 'Effect of water vapour on cyclic oxidation of Fe-Cr alloys', Materials and Corrosion - Werkstoffe und Korrosion, vol. 62, pp. 496 - 503, http://dx.doi.org/10.1002/maco.201005866
2011
Young DJ; Zhang J; Geers C; Schutz M, 2011, 'Recent Advances in Understanding Metal Dusting - A Review', Materials and Corrosion - Werkstoffe und Korrosion, vol. 62, pp. 7 - 28, http://dx.doi.org/10.1002/maco.201005675
2011
Li H; Zhang J; Young DJ, 2011, 'Oxidation of Fe-Si alloys in CO2-H2O atmospheres', Materials at High Temperatures, vol. 28, pp. 297 - 301, http://dx.doi.org/10.3184/096034011X13185202328867
2011
Gheno T; Monceau D; Zhang J; Young DJ, 2011, 'Carburisation of ferritic Fe-Cr alloys by low carbon activity gases', Corrosion Science, vol. 53, pp. 2767 - 2777, http://dx.doi.org/10.1016/j.corsci.2011.05.013
2011
Gheno T; Li H; Zhang J; Young DJ, 2010, 'High Temperature Corrosion of Fe-Cr, Fe-Al, Fe-Si and Fe-Si-Al Alloys in CO2-H2O Gases', Materials Science Forum, vol. 654-656, pp. 1948 - 1951, http://dx.doi.org/10.4028/www.scientific.net/MSF.654-656.1948
2010
Al Motin M; Zhang J; Young DJ, 2010, 'Simultaneous Oxidation and Metal Dusting of Fe-Si Alloys', ECS Transactions, vol. 25, pp. 57 - 69, http://dx.doi.org/10.1149/1.3315796
2010
Motin MAA; Zhang J; Young DJ, 2010, 'Simultaneous Corrosion of Fe-Si Alloys by Carbon and Oxygen', Journal of the Electrochemical Society, vol. 157, pp. C375 - C381, http://dx.doi.org/10.1149/1.3481563
2010
Li Q; Peng X; Zhang J; Zong GX; Wang FH, 2010, 'Comparison of the oxidation of high-sulfur Ni–25Cr–5Al alloys in as-cast and as-sputtered states', Corrosion Science, vol. 52, pp. 1213 - 1221, http://dx.doi.org/10.1016/j.corsci.2009.12.005
2010
Wu Q; Zhang J; Sun Y, 2010, 'Oxidation behavior of TiC particle-reinforced 304 stainless steel', Corrosion Science, vol. 52, pp. 1003 - 1010, http://dx.doi.org/10.1016/j.corsci.2009.11.025
2010
Othman NK; Zhang J; Young DJ, 2010, 'Water Vapour Effects on Fe–Cr Alloy Oxidation', Oxidation of Metals, vol. 73, pp. 337 - 352, http://dx.doi.org/10.1007/s11085-009-9183-9
2010
Speck P; Young DJ; Zhang J, 2010, 'Metal Dusting of Nickel–Aluminium Alloys', Oxidation of Metals, vol. 73, pp. 255 - 274, http://dx.doi.org/10.1007/s11085-009-9178-6
2010
Othman NK; Zhang J; Young DJ, 2010, 'Temperature and Water Vapour Effects on the Cyclic Oxidation Behavior of Fe-Cr alloys', Corrosion Science, vol. 52, pp. 2827 - 2836, http://dx.doi.org/10.1016/j.corsci.2010.04.026
2010
Othman NK; Othman O; Zhang J; Young DJ, 2010, 'Water vapour effects of cyclic oxidation on Fe-Cr Alloys', Sains Malaysiana, vol. 39, pp. 249 - 259
2010
Motin MAA; Zhang J; Munroe PR; Young DJ, 2010, 'Internal Oxidation and Metal Dusting of Fe-Si Alloys', Corrosion Science, vol. 52, pp. 3280 - 3286, http://dx.doi.org/10.1016/j.corsci.2010.05.045
2010
Motin MAA; Zhang J; Young DJ, 2010, 'Simultaneous Internal Oxidation and Metal Dusting of Fe-Si Alloys', ECS Transactions, vol. 25, pp. 57 - 69
2010
Othman NK; Zhang J; Young DJ, 2009, 'Kinetic and microstructural analyses of chromia forming alloys during cyclic oxidation', Journal of the Chinese Society of Corrosion and Protection, vol. 29, pp. 315
2009
Zhang J; Young DJ, 2009, 'Metal Dusting - Mechanisms and Preventions', Journal of the Chinese Society of Corrosion and Protection, vol. 29, pp. 262 - 276
2009
Young DJ; Al Motin M; Zhang J, 2009, 'Diffusion in Metal Dusting Processes', Defect and Diffusion Forum, vol. 289-292, pp. 289 - 292, http://dx.doi.org/10.4028/www.scientific.net/DDF.289-292
2009
Young DJ; Zhang J, 2009, 'Understanding Metal Dusting Mechanisms in Terms of Reaction Morphologies', ECS Transactions, vol. 16, pp. 3 - 15
2009
Yin H; Zhang J; Young DJ, 2009, 'Effect of gas composition on coking and metal dusting of 2.25Cr-1Mo steel compared with iron', Corrosion Science, vol. 51, pp. 2983 - 2993, http://dx.doi.org/10.1016/j.corsci.2009.08.026
2009
Young DJ; Motin MAA; Zhang J, 2009, 'Diffusion in metal dusting processes', Defect and Diffusion Forum, vol. 289-292, pp. 51 - 62, http://dx.doi.org/10.4028/www.scientific.net/DDF.289-292.51
2009
Zhang J; Kong CH; Young DJ, 2009, 'Surface orientation effects on initial carbon deposition and metal dusting of nickel', Materials at High Temperatures, vol. 26, pp. 45 - 55, http://dx.doi.org/10.3184/096034009X438176
2009
Othman NK; Othman N; Zhang J; Young DJ, 2009, 'Effects of water vapour on isothermal oxidation of chromia-forming alloys in Ar/O2 and Ar/H2 atmospheres', Corrosion Science, vol. 51, pp. 3039 - 3049, http://dx.doi.org/10.1016/j.corsci.2009.08.032
2009
Zhang J; Boddington K; Young DJ, 2008, 'Oxidation, carburisation and metal dusting of 304 stainless steel in CO/CO2 and CO/H2/H2O gas mixtures', Corrosion Science, vol. 50, pp. 3107 - 3115, http://dx.doi.org/10.1016/j.corsci.2008.08.017
2008
Zhang J; Young DJ, 2008, 'Coking and dusting of Fe-Ni alloys in CO-H2-H2O gas mixtures', Oxidation of Metals, vol. 70, pp. 189 - 211, http://dx.doi.org/10.1007/s11085-008-9115-0
2008
Zhang J; Safarzadeh M; Young DJ, 2008, 'Carbon permeability of nickel and Ni-Cu alloys', Oxidation of Metals, vol. 70, pp. 15 - 24, http://dx.doi.org/10.1007/s11085-008-9108-z
2008
Zhang J; Munroe PR; Young DJ, 2008, 'Microprocesses in nickel accompanying metal dusting', ACTA Materialia, vol. 56, pp. 68 - 77, http://dx.doi.org/10.1016/j.actamat.2007.09.010
2008
Zhang J; Schneider A; Inden G, 2008, 'Initiation and growth of iron metal dusting in CO-H2-H2O gas mixtures', Corrosion Science, vol. 50, pp. 1020 - 1034, http://dx.doi.org/10.1016/j.corsci.2007.11.021
2008
Zhang J; Young DJ, 2007, 'Metal Dusting of Nickel and its Alloys', ECS Transactions, vol. 3, pp. 27 - 41, http://dx.doi.org/10.1149/1.2721457
2007
Longbottom R; Ostrovski O; Zhang J; Young DJ, 2007, 'The Stability of cementite formed from hematite and titanomagnetite ore', Metallurgical and Materials Transactions B - Process Metallurgy and Materials Processing Science, vol. 38, pp. 175 - 184, http://dx.doi.org/10.1007/s11663-006-9005-2
2007
Zhang J; Young DJ, 2007, 'Kinetics and mechanisms of nickel metal dusting I: Kinetics and morphology', Corrosion Science, vol. 49, pp. 1496 - 1512, http://dx.doi.org/10.1016/j.corsci.2006.08.008
2007
Zhang J; Young DJ, 2007, 'Effect of copper on metal dusting of austenitic stainless steels', Corrosion Science, vol. 49, pp. 1450 - 1467, http://dx.doi.org/10.1016/j.corsci.2006.06.032
2007
Zhang J; Cole DM; Young DJ, 2005, 'Alloying with copper to reduce metal dusting of nickel', Materials and Corrosion - Werkstoffe und Korrosion, vol. 56, pp. 756 - 764, http://dx.doi.org/10.1002/maco.200503876
2005
Schneider A; Zhang J, 2005, 'Orientation relationship between a ferritic matrix and kappa -phase (Fe3ALCx) precipitates formed during metal dusting of Fe- 15Al', Intermetallics, vol. 13, pp. 1332 - 1336, http://dx.doi.org/10.1016/j.intermet.2005.02.008
2005
Zhang J; Schneider A; Inden G, 2004, 'Cementite Decomposition and Coke Gasification in He and H2-He Gas Mixtures', Corrosion Science, vol. 46, pp. 667 - 679, http://dx.doi.org/10.1016/S0010-938X(03)00177-X
2004
Zhang J; Schneider A; Inden G, 2003, 'Characterisation of the Coke Formed during Metal Dusting of Iron in CO-H2-H2O Gas Mixtures', Corrosion Science, vol. 45, pp. 1329 - 1341, http://dx.doi.org/10.1016/S0010-938X(02)00251-2
2003
Zhang J; Schneider A; Inden G, 2003, '¡§ƒÑ-Fe Layer Formation during Metal Dusting of Iron in CO-H2-H2O Gas Mixtures', Materials and Corrosion - Werkstoffe und Korrosion, vol. 54, pp. 763 - 769
2003
Zhang J; Schneider A; Inden G, 2003, 'Metal Dusting of Iron in CO-H2-H2O Gas Mixtures at 600„aC', Journal of Corrosion Science and Engineering, vol. 6, pp. H057
2003
Schneider A; Zhang J; Inden G, 2003, 'Metal Dusting of binary Fe-Al alloys in CO-H2-H2O Mixtures', Journal of Corrosion Science and Engineering, vol. 6, pp. H043
2003
Zhang J; Schneider A; Inden G, 2003, 'Coke Formation during Metal Dusting of Iron in CO-H2-H2O Gas with High CO Content', Materials and Corrosion - Werkstoffe und Korrosion, vol. 54, pp. 770 - 777, http://dx.doi.org/10.1002/maco.200303741
2003
Schneider A; Zhang J, 2003, 'Metal Dusting of Ferritic Fe-Al-M-C (M = Ti, V, Nb, Ta) Alloys in CO-H2-H2O Gas Mixtures at 650 „aC', Materials and Corrosion - Werkstoffe und Korrosion, vol. 54, pp. 778 - 784, http://dx.doi.org/10.1002/maco.200303739
2003
Zhang J; Schneider A; Inden G, 2003, 'Effect of Gas Composition on Cementite Decomposition and Coke Formation on Iron', Corrosion Science, vol. 45, pp. 281 - 299, http://dx.doi.org/10.1016/S0010-938X(02)00092-6
2003
Zhang J; Schneider A; Inden G, 2003, 'α-Fe layer formation during metal dusting of iron in CO-H 2-H2O gas mixtures', Materials and Corrosion, vol. 54, pp. 763 - 769, http://dx.doi.org/10.1002/maco.200303740
2003
Zhang J; Ostrovski O, 2002, '., Iron Ore Reduction/Cementation: Experimental Results and Kinetic Modelling', Ironmaking and Steelmaking, vol. 29, pp. 15 - 21, http://dx.doi.org/10.1179/030192302225001929
2002
Zhang J; Grabke HJ; Müller-Lorenz E, 2002, 'Inhibiting the reoxidation of directly reduced iron by vapour phase inhibitors', Steel Research, vol. 73, pp. 421 - 427, http://dx.doi.org/10.1002/srin.200200009
2002
Ostrovski O; Zhang J, 2001, 'Effect of Sulphur on Iron Carbide Formation and Stability', ISIJ International, vol. 41, pp. 340 - 344, http://dx.doi.org/10.2355/isijinternational.41.340
2001
Zhang J; Ostrovski O; Suzuki K, 2000, 'Effect of Temperature on Cementite Formation by Reaction of Iron Ore with H2-CH4-Ar Gas,', Metallurgical and Materials Transactions B - Process Metallurgy and Materials Processing Science, vol. 31, pp. 1139 - 1142, http://dx.doi.org/10.1007/s11663-000-0091-2
2000
Zhang JQ; Wu BY; Hu Z; Wang GQ, 1997, 'Mechanical alloying effect on the structure of Fe-Al-(Si) alloy', JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, vol. 13, pp. 219 - 222, http://gateway.webofknowledge.com/gateway/Gateway.cgi?GWVersion=2&SrcApp=PARTNER_APP&SrcAuth=LinksAMR&KeyUT=WOS:A1997WX54700011&DestLinkType=FullRecord&DestApp=ALL_WOS&UsrCustomerID=891bb5ab6ba270e68a29b250adbe88d1
1997
Conference Papers
add
Xi X; Zhang J; Young DJ, 2020, 'Effect of cyclic reaction on corrosion behaviour of chromiaforming alloys in CO2-rich gas at 650°C', in Corrosion and Prevention 2019
2020
Xi X; Zhang J; Young DJ, 2020, 'Effect of cyclic reaction on corrosion behaviour of chromiaforming alloys in CO2-rich gas at 650°C', in Corrosion and Prevention 2019
2020
Aye KK; Zhang J; Young DJ, 2018, 'Chlorine-induced corrosion of chromia forming alloys in wet CO2 atmospheres at 650 °C', in Corrosion and Prevention 2018
2018
Yang J; Zhang J; Ostrovski O; Zhang C; Cai D, 2018, 'Flux-steel reaction of CaO-SiO 2 and CaO-Al 2 O 3 -based mold fluxes with high-al steel', in ICS 2018 - 7th International Congress on Science and Technology of Steelmaking: The Challenge of Industry 4.0
2018
Yuan X; Wang L; Zhang J; Sasaki Y; Ostrovski O; Zhang C; Cai D, 2018, 'Analysis of viscosity of fluorine-free mould fluxes', in ICS - 2018, ICS 2018, Associazione Italiana di Metallurgia, Venice, Italy, pp. 1 - 10, presented at ICS 2018, Venice, Italy, 13 June 2018 - 15 June 2018
2018
Kapelyushin Y; Sasaki Y; Zhang J; Ostrovski O, 2018, 'A study of cementite formation in the reduction of hematite by CO-CO2 gas mixture using high temperature XRD', in Davis B (ed.), Extraction 2018 Proceedings of the First Global Conference on Extractive Metallurgy, Springer, Ottawa, Canada, pp. 683 - 695, presented at First Global Conference on Extractive Metallurgy, Ottawa, Canada, 26 August 2018 - 29 August 2018, http://dx.doi.org/10.1007/978-3-319-95022-8_54
2018
Concepcion C; Hsu Y-L; Xie Y; Zhang J, 2018, 'CORROSION BEHAVIOUR OF NI-CR ALLOYS IN OXYGEN AT HIGH TEMPERATURE', in Corrosion & prevention 2018, Australasian Corrosion Association, Adelaide, pp. 1 - 10, presented at Corrosion & Prevention 2018, Adelaide, 11 November 2018 - 14 November 2018
2018
Aye KK; Zhang J; Young D, 2018, 'CHLORINE-INDUCED CORROSION OF CHROMIA FORMING ALLOYS IN WET CO2 ATMOSPHERES AT 650⁰C', in Corrosion & Prevention 2018, Australian Corrosion Association, Adelaide, pp. 1 - 11, presented at Corrosion & Prevention 2018, Adelaide, 11 November 2018 - 14 November 2018
2018
Yang J; Zhang J; Ostrovski O; Zhang C; Cai D, 2018, 'Flux-Steel Reaction of CaO-SiO2 and CaO-Al2O3-based Mold Fluxes with High-Al Steel', in ICS 2018, ICS 2018, Associazione Italiana di Metallurgia, Venice Italy, pp. 1 - 9, presented at ICS 2018, Venice Italy, 13 June 2018 - 15 June 2018
2018
Nguyen TD; Zhang J; Young DJ, 2017, 'Effects of Ti and Al on corrosion of Ni-20Cr and Ni-30Cr alloys in dry CO2 gas', in Corrosion and Prevention 2017
2017
Xie Y; Zhang J; Young D, 2017, 'Effect of water vapour on oxidation behaviour of Ni-Cr alloys in CO2 atmosphere at 650°c', in Australasian Corrosion Association Annual Conference - 2017, Australasian Corrosion Association, Sydney, Australia, pp. 1 - 12, presented at Corrosion & Prevention 2017, Sydney, Australia, 12 November 2017 - 15 November 2017
2017
Li M; Zhou C; Zhang J; Young D, 2017, 'Effect of Ni-Re diffusion barrier on Ni-Al coating structure and its oxidation in dry CO2 gas at 650⁰C', in Corrosion & Prevention 2017, Australasian Corrosion Association, Sydney, Australia, pp. 1 - 7, presented at Corrosion & Prevention 2017, Sydney, Australia, 12 November 2017 - 15 November 2017
2017
Zhang J; Naing T; Nguyen T; Young D, 2016, 'Corrosion behaviour of some commercial alloys in co2 gas at high temperature', in Proceedings of Corrosion & Prevention 2016, Australasian Corrosion Association, Auckland, NZ, pp. 1 - 7, presented at Corrosion & Prevention 2016, Auckland, NZ, 13 November 2016 - 16 November 2016
2016
Xie Y; Zhang J; Young DJ, 2016, 'Effect of temperature on oxidation behaviour of Ni-Cr alloys in CO2 atmosphere', in ECS Transactions, pp. 19 - 35, http://dx.doi.org/10.1149/07528.0019ecst
2016
Wang L; Zhang J; Sasaki Y; Ostrovski O; Zhang C; Cai D, 2016, 'Stability of fluorine-free mould fluxes Sio2-Cao-Al2O3-B2O3-Na2O for steel continuous casting', in Advances in Molten Slags, Fluxes, and Salts: Proceedings of the 10th International Conference on Molten Slags, Fluxes and Salts 2016, pp. 1319 - 1326, http://dx.doi.org/10.1007/978-3-319-48769-4_143
2016
Yang J; Zhang J; Sasaki Y; Ostrovski O; Zhang C; Cai D; Kashiwaya Y, 2016, 'Effect of Na2O on Crystallisation Behaviour and Heat Transfer of Fluorine-free Mould Fluxes', in Reddy R; Chaubal P; Pistorius C; Pal U (eds.), Proceedings of the 10th International Conference on Molten Slags, Fluxes and Salts, John Wiley & Sons, Inc., Hoboken, New Jersey, Seattle, USA, pp. 335 - 342, presented at The 10th International Conference on Molten Slags, Fluxes and Salts, Seattle, USA, 22 May 2016 - 25 May 2016
2016
Wang L; Zhang J; Sasaki Y; Ostrovski O; Zhang C; Cai D, 2016, 'Stability of Fluorine-free Mould Fluxes SiO2-CaO-Al2O3-B2O3-Na2O for Steel Continuous Casting', in Reddy R; Chaubal P; Pistorius C; Pal U (eds.), Proceedings of the 10th International Conference on Molten Slags, Fluxes and Salts, John Wiley & Sons, Inc., Hoboken, New Jersey, Seattle, USA, pp. 1319 - 1326, presented at The 10th International Conference on Molten Slags, Fluxes and Salts, Seattle, USA, 22 May 2016 - 25 May 2016
2016
Wang L; Cui Y; Zhang C; Cai D; Zhang J; Sasaki Y; Ostrovski O, 2015, 'Melting properties and viscosity of the SiO2-CaO-Al2O3-B2O3-MxOy (MxOy: Na2O, TiO2, or MgO) system', in Proceedings of the 6th International Congress on the Science and Technology of Steelmaking, ICS 2015, pp. 622 - 625
2015
Nguyen T; Zhang J; Young D, 2015, 'Effect of Mn on corrosion of Fe-Cr and Fe-Cr-Ni alloys in dry CO2 at 650C', in Corrosion and Prevention 2015, Adelaide, presented at Corrosion and Prevention 2015, Adelaide, 15 November 2015 - 18 November 2015
2015
McCarroll I; La Fontaine A; Felfer P; Zhang J; Young D; Cairney J, 2015, 'Atom probe microscopy of oxidation products', in European Corrosion Congress, EUROCORR 2015, pp. 571
2015
Yang J; Sasaki Y; Zhang J; Ostrovski O; Kashiwaya Y; Zhang C; Cai D, 2015, 'A study of the effect of CaO/SiO2 ratio on the crystallisation behaviour of fluoride-free mould fluxes using single and double hot thermocouple techniques', in Proceedings of the 6th International Congress on the Science and Technology of Steelmaking, ICS 2015, pp. 610 - 613
2015
Jullian D; Prillieux A; Zhang J; Hibbert D; Young D, 2015, 'Oxygen solubility in Fe-Ni alloys at high temperature in Rhines packs and in gas mixtures', in Corrosion and Prevention 2015, Australasian Corrosion Association, Adelaide, presented at Corrosion and Prevention 2015, Adelaide, 15 November 2015 - 18 November 2015
2015
Yu C; Young DJ; Zhang J, 2015, 'Corrosion behaviour of ferritic Fe-Cr alloys in CO2-H2O-SO2 GASES at 800°C', in Australasian Corrosion Association Annual Conference: Corrosion and Prevention 2015, ACA 2015
2015
Yu C; Zhang J; Young D, 2015, 'Corrosion behavior of ferritic Fe-Cr alloys in CO2-H2O-SO2 gases at 800C', in Corrosion and Prevention 2015, Australasian Corrosion Association, Adelaide, presented at Corrosion and Prevention 2015, Adelaide, 15 November 2015 - 18 November 2015
2015
Yu C; Nguyen TD; Zhang J; Young DJ, 2015, 'Effect of sulphur on Fe-20Cr-(Mn, Si) and Fe-20Ni-20Cr-(Mn, Si) corrosion in CO2-H2O at 650°C', in ECS Transactions, pp. 23 - 39, http://dx.doi.org/10.1149/06618.0023ecst
2015
Nguyen TD; Zhang J; Young DJ, 2014, 'Effect of Mn on corrosion of Fe-Cr and Fe-Cr-Ni alloys in dry and wet CO2 gas', in Corrosion & Prevention 2014, Corrosion & Prevention 2014, Darwin, Australia, presented at Corrosion & Prevention 2014, Darwin, Australia, 21 September 2014 - 24 September 2014
2014
Nguyen T; Zhang J; Young D, 2014, 'Effect of Mn on Corrosion of Fe-Cr and Fe-Cr-Ni alloys in dry and wet CO2 gas mixtures at high tempeature', in Corrosion & Prevention 2014, Australia, presented at Corrosion & Prevention 2014, Australia, 21 September 2014 - 24 September 2014
2014
Yu C; Zhang J; Young DJ, 2014, 'Effect of sulphur on Fe-9Cr-(Mn, Si) alloy corrosion in CO2-H2O gas at 650C', in Corrosion & Prevention 2014, Darwin, Australia, presented at Corrosion & Prevention 2014, Darwin, Australia, 21 September 2014 - 24 September 2014
2014
Nguyen TD; Zhang J; Young D, 2014, 'Effect of Si on Corrosion of Fe-Cr and Fe-Cr-Ni alloys in wet CO2 gas', in 19th International corrosion congress, 19th International corrosion congress, South Korea, presented at 19th International corrosion congress, South Korea, 02 November 2014 - 06 November 2014
2014
Young DJ; Zhang J, 2013, 'Carbon corrosion of alloys at high temperature', in Journal of the Southern African Institute of Mining and Metallurgy, South African Institute of Mining and Metallurgy, pp. 149 - 154, http://www.saimm.co.za/Journal/v113n02p149.pdf
2013
Xiang Z; Zhang J; Kong C; Peng X; Young DJ, 2013, 'Metal dusting of sputtered NiCr nanocrytalline coating in CO-H2-H2O gas', in Annual Conference of the Australasian Corrosion Association 2013: Corrosion and Prevention 2013, pp. 249 - 257
2013
Nguyen DT; Zhang J; Young D, 2013, 'OXIDATION OF Fe-Cr-Si AND Fe-Cr-Ni-Si ALLOYS IN DRY CO2 GAS', in Proceedings Corrosion & Prevention 2013, Brisbane, Australia, pp. 184 - 189, presented at Corrosion & Prevention 2013, Brisbane, Australia, 10 November 2013 - 13 November 2013
2013
Xiang Z; Zhang J; Kong C; Peng X; Young D, 2013, 'METAL DUSTING OF SPUTTERED NiCr NANOCRYTALLINE COATING IN CO-H2-H2O GAS', in Proceedings of Corrosion & Prevention 2013, Australasian Corrosion Association, Brisbane, pp. 1 - 9, presented at Corrosion & Prevention 2013, Brisbane, 10 November 2013 - 13 November 2013
2013
Slabbert G; Mulaudzi F; Cornish L; Papo J; Morudu V; Zhang J, 2012, 'THE EFFECT OF THE MATRIX STRUCTURE ON THE METAL DUSTING RATE IN HYDOCARBON ENVIRONMENTS', in Proceedings of the AMI Ferrous 2012 Conference, The Southern African Institute of Mining and Metallurgy, Mount Grace Country House & Spa, Magaliesburg, pp. 1 - 17, presented at Ferrous and Base Metals Development Network Conference 2012, Mount Grace Country House & Spa, Magaliesburg, 15 October 2012 - 17 October 2012
2012
Mulaudzi F; Cornish L; Slabbert G; Papo J; Zhang J, 2012, 'AN INVESTIGATION OF METAL DUSTING CORROSION ON Fe- AND Ni-BASED ALLOYS', in Proceedings of the AMI Ferrous 2012 Conference, The Southern African Institute of Mining and Metallurgy, Mount Grace Country House & Spa, Magaliesburg, pp. 1 - 15, presented at Ferrous and Base Metals Development Network Conference 2012, Mount Grace Country House & Spa, Magaliesburg, 15 October 2012 - 17 October 2012
2012
Zhang J; Li H; Kong CH; Young DJ, 2012, 'Carburisation of Fe-Al alloys in high and low carbon activity gases at high temperatures', in Annual Conference of the Australasian Corrosion Association 2012, Melbourne, VIC., pp. 91 - 100, presented at Annual Conference of the Australasian Corrosion Association 2012, Melbourne, VIC., 11 November 2012 - 14 November 2012
2012
Li H; Zhang J; Young DJ, 2012, 'Temperature effect on oxidation of binary Fe-Si and Fe-Al alloys in CO2-H2O gas atmosphere', in Annual Conference of the Australasian Corrosion Association 2012, Melbourne, VIC., pp. 80 - 90, presented at Annual Conference of the Australasian Corrosion Association 2012, Melbourne, VIC., 11 November 2012 - 14 November 2012
2012
Mulaudzi F; Cornish L; Slabbert G; Papo J; Zhang J, 2012, 'An investigation of metal dusting corrosion of alloys N06025 and N08800', in NACE - International Corrosion Conference Series, Salt Lake City, UT, pp. 1559 - 1573, presented at Corrosion 2012, Salt Lake City, UT, 11 March 2012 - 15 March 2012, http://dx.doi.org/
2012
Mulaudzi FML; Cornish LA; Slabbert GA; Papo MJ; Zhang J, 2012, 'A study of metal dusting corrosion on Fe- and Ni-based alloys', in JOURNAL OF THE SOUTHERN AFRICAN INSTITUTE OF MINING AND METALLURGY, SOUTHERN AFRICAN INST MINING METALLURGY, Johannesburg, SOUTH AFRICA, pp. 123 - 130, presented at Ferrous and Base Metals Development Network Conference, Johannesburg, SOUTH AFRICA, 15 October 2012 - 17 October 2012, http://gateway.webofknowledge.com/gateway/Gateway.cgi?GWVersion=2&SrcApp=PARTNER_APP&SrcAuth=LinksAMR&KeyUT=WOS:000320295800011&DestLinkType=FullRecord&DestApp=ALL_WOS&UsrCustomerID=891bb5ab6ba270e68a29b250adbe88d1
2012
Zhang J; Young DJ, 2012, 'Effect of Copper on the Dusting of Fe-Ni Alloys', in ECS Transactions, The Electrochemical Society, USA, pp. 37 - 46, presented at 221st Electrochemical Society Meeting, Seattle, WA USA, 06 May 2012 - 10 May 2012, http://dx.doi.org/10.1149/1.4717998
2012
Slabbert G; Mulaudzi F; Cornish L; Papo J; Zhang J, 2012, 'The Effect of Carbide-Forming Elements on the Metal Dusting Rate in Hydocarbon Environments', in Proceedings of the Australian Corrosion Association, Corrosion and Prevention 2012, Melbourne, pp. 1 - 12, presented at Corrosion and Prevention 2012, Melbourne
2012
Zhang J; Peng X; Young DJ; Wang F, 2012, 'Cyclic Oxidation Resistance of Nano-crystalline 304 Stainless Steel', in Proceedings of Corrosion Prevention and Environment Protection of Materials for a New Era, The Corrosion Engineering Association of the Republic of China, Kaohsiung, Taiwan, pp. 1 - 7, presented at 16th APCCC, Kaohsiung, Taiwan, 21 October 2012 - 24 October 2012
2012
Mulaudzi FML; Cornish LA; Slabbert GA; Mahlangu FM; Zhang J, 2011, 'On the metal dusting corrosion of Alloy 800 ferrules in a petrochemical environment', in 18th International Corrosion Congress 2011, pp. 1485 - 1493
2011
Zhang J; Othman NK; Young DJ, 2011, 'Water vapour effect on cyclic oxidation of Fe-Cr alloys at 950°C', in 18th International Corrosion Congress 2011, pp. 806 - 814
2011
Li H; Munroe PR; Zhang J; Young DJ, 2011, 'THE TRANSITION FROM INTERNAL TO PROTECTIVE OXIDATION DURING OXIDATION OF DILUTE FE-AL ALLOYS IN AR-20% CO2', in Proceedings of the Australian Corrosion Association, 18th International Corrosion Congress 2011, Perth, WA, Australia, pp. 1 - 9, presented at 18th International Corrosion Congress 2011, Perth, WA, Australia, 20 November 2011 - 24 November 2011
2011
Mulaudzi F; Cornish L; Slabbert G; Mahlangu F; Zhang J, 2011, 'ON THE METAL DUSTING CORROSION OF ALLOY 800 FERRULES IN A PETROCHEMICAL ENVIRONMENT', in Proceedings of the Australian Corrosion Association, 18th International Corrosion Congress 2011, Perth, WA, Australia, pp. 1 - 9, presented at 18th International Corrosion Congress 2011, Perth, WA, Australia, 20 November 2011 - 24 November 2011
2011
Li H; Munroe P; Zhang J; Young DJ, 2011, 'The transition from internal to protective oxidation during oxidation of dilute Fe-Al alloys in Ar- 20% CO 2', in 18th International Corrosion Congress 2011, pp. 865 - 873
2011
Gheno T; Zhang J; Young DJ, 2011, 'HIGH TEMPERATURE CORROSION OF CHROMIA-FORMING ALLOYS UNDER OXYFUEL FIRING CONDITIONS', in Proceedings of the Australian Corrosion Association, 18th International Corrosion Congress 2011, Perth, WA, Australia, pp. 1 - 9, presented at 18th International Corrosion Congress 2011, Perth, WA, Australia, 20 November 2011 - 24 November 2011
2011
Zhang J; Othman NK; Young DJ, 2011, 'WATER VAPOUR EFFECT ON CYCLIC OXIDATION OF FE-CR ALLOYS AT 950¢XC', in Proceedings of the Australian Corrosion Association, 18th International Corrosion Congress 2011, Perth, WA, Australia, pp. 1 - 9, presented at 18th International Corrosion Congress 2011, Perth, WA, Australia, 20 November 2011 - 24 November 2011
2011
Gheno T; Zhang J; Young DJ, 2010, 'HIGH TEMPERATURE CORROSION RESISTANCE OF Fe-Cr-Ni ALLOYS IN CO2-H2O', in Proceedings of the Australian Corrosion Association, Corrosion & Prevention 2010, Adelaide, pp. 1 - 9, presented at Corrosion & Prevention 2010, Adelaide
2010
Li H; Zhang J; Young DJ, 2010, 'Oxidation properties of Fe-Al alloys in CO 2-H 2O gas atmosphere', in 50th Annual Conference of the Australasian Corrosion Association 2010: Corrosion and Prevention 2010, pp. 306 - 317
2010
Zhang J; Young DJ, 2010, 'EFFECTS OF COPPER ON COKING AND DUSTING OF Fe-Ni ALLOYS', in Proceedings of the Australian Corrosion Association, Corrosion & Prevention 2010, Adelaide, pp. 1 - 13, presented at Corrosion & Prevention 2010, Adelaide
2010
Zhang J; Young DJ, 2010, 'Effects of copper on coking and dusting of Fe-Ni alloys', in 50th Annual Conference of the Australasian Corrosion Association 2010: Corrosion and Prevention 2010, pp. 215 - 227
2010
Li H; Zhang J; Young DJ, 2010, 'OXIDATION PROPERTIES OF FE-AL ALLOYS IN CO2-H2O GAS ATMOSPHERE', in Proceedings of the Australian Corrosion Association, Corrosion & Prevention 2010, Adelaide, pp. 1 - 12, presented at Corrosion & Prevention 2010, Adelaide
2010
Gheno T; Zhang J; Young DJ, 2010, 'High temperature corrosion resistance of Fe-Cr-Ni alloys in CO 2-H 2O', in 50th Annual Conference of the Australasian Corrosion Association 2010: Corrosion and Prevention 2010, pp. 384 - 392
2010
Li H; Zhang J; Young DJ, 2009, 'Oxidation behaviours of Fe-Al, Fe-Si and Fe-Si-Al alloys in CO2-containing gas atmosphere', in 49th Annual Conference of the Australasian Corrosion Association 2009: Corrosion and Prevention 2009, pp. 505 - 512
2009
Gheno T; Zhang J; Young DJ, 2009, 'High temperature corrosion of Fe-Cr alloys in CO2-H2O gas atmospheres', in Proceedings of the Australian Corrosion Association, Coffs Harbour, pp. 403 - 413, presented at Corrosion & Prevention 2009, Coffs Harbour, 15 November 2009 - 19 November 2009
2009
Speck P; Young DJ; Zhang J, 2009, 'Carburisation of gammar-phase nickel-aluminum-hafnium alloys', in Proceedings of the Australian Corrosion Association, Coffs Harbour, pp. 142 - 151, presented at Corrosion & Prevention 2009, Coffs Harbour, 15 November 2009 - 19 November 2009
2009
Zhang J; Wu Q; Young DJ, 2009, 'METAL DUSTING OF NICKEL- AND COBALT-BASE ALLOYS', in Proceedings of the Australian Corrosion Association, Coffs Harbour, pp. 483 - 493, presented at Corrosion Control 2009, Coffs Harbour
2009
Li H; Zhang J; Young DJ, 2009, 'Oxidation behavior of Fe-Al, Fe-Si and Fe-Al-Si alloys in CO2 gas atmosphere', in Proceedings of the Australian Corrosion Association, Corrosion & Prevention 2009, Coffs Harbour, presented at Corrosion & Prevention 2009, Coffs Harbour, 15 November 2009 - 19 November 2009
2009
Young DJ; Zhang J; Othman NK, 2008, 'Kinetic and microstructural analysis of chromia forming alloys during cyclic oxidation', in Proceedings of Corrosion and Prevention 2008, Wellington, New Zealand, pp. 485 - 495, presented at Corrosion and Prevention 2008, Wellington, New Zealand, 16 November 2008 - 19 November 2008
2008
Young DJ; Zhang J, 2008, 'Corrosion behaviour of 304 Stainless Steel in Carburizing Gas Atmospheres', in Proceedings of Corrosion and Prevention 2008, Wellington, New Zealand, pp. 218 - 228, presented at Corrosion and Prevention 2008, Wellington, New Zealand, 16 November 2008 - 19 November 2008
2008
Young DJ; Zhang J, 2008, 'Understanding metal dusting mechanisms', in ECS Transactions, pp. 3 - 15, http://dx.doi.org/10.1149/1.3224738
2008
Zhang J; Young DJ; Othman NK, 2007, 'Steam Effects on Cyclic Oxidation of Chromia Forming Alloys', in Corrosion Control 007 Conference, Sydney, pp. 864 - 875, presented at Corrosion Control 007, Sydney, 25 November 2007 - 28 November 2007
2007
Zhang J; Young DJ, 2007, 'Composition effects in metal dusting of Fe-Ni alloys', in 47th Annual Conference of the Australasian Corrosion Association 2007: Corrosion Control 2007, pp. 138 - 145
2007
Zhang J; Young DJ; Munroe PR; Brady MP; Al Motin M, 2007, 'Effects of Alloy Additions on Metal Dusting of Iron', in Corrosion Control 007 Conference, Sydney, pp. 369 - 378, presented at Corrosion Control 007, Sydney, 25 November 2007 - 28 November 2007
2007
Zhang J; Young DJ; Yin H, 2007, 'Metal dusting of 2.25Cr-1Mo IN CO-H2-H20', in Corrosion Control 007 Conference, Sydney, pp. 614 - 623, presented at Corrosion Control 007, Sydney, 25 November 2007 - 28 November 2007
2007
Zhang J; Young DJ, 2007, 'Alloy Composition Effects in Metal Dusting of Fe-Ni alloys', in Corrosion Control 007 Conference, Corrosion Control 007, Sydney, presented at Corrosion Control 007, Sydney, 25 November 2007 - 28 November 2007
2007
Zhang J; Young DJ, 2006, 'The use of Copper to Prevent Dusting of Stainless Steels', in Corrosion and Prevention, Hobart, pp. 613 - 620, presented at Corrosion and Prevention 2006, Hobart, 19 November 2006 - 22 November 2006
2006
Longbottom R; Ostrovski O; Zhang J; Young DJ, 2006, 'Formation of cementite in reduction of titanomagnetite ore and cementite stability', in Proceedings of 4th International Congress on the Science and Technology of Ironmaking, Osaka, Japan, pp. 73 - 76, presented at 4th International Congress on the Science and Technology of Ironmaking, Osaka, Japan, 26 November 2006 - 30 November 2006
2006
Zhang J; Young DJ, 2006, 'COPPER EFFECT ON METAL DUSTING OF 304 AND 310 STAINLESS STEELS', in COPPER EFFECT ON METAL DUSTING OF 304 AND 310 STAINLESS STEELS, Asian-Pacific Materials & Corrosion Association, Shanghai China, presented at 14th Asian-Pacific Corrosion Control Conference, Shanghai China, 21 October 2006 - 24 October 2006
2006
Zhang J; Young DJ, 2005, 'Metal Dusting and its Prevention', in Proceedings of the Australian Corrosion Association, Gold Coast, Qld, pp. 438 - 447, presented at Corrosion and Prevention 2005, Gold Coast, Qld, 20 November 2005 - 23 November 2005
2005
Zhang J; Young DJ, 2005, 'EFFECT OF COPPER ON METAL DUSTING OF IRON', in EFFECT OF COPPER ON METAL DUSTING OF IRON, Chinese Society for Corrosion and Protection, Beijing China, presented at 16th International Corrosion Congress, Beijing China
2005
Schneider A; Zhang J; Inden G, 2003, 'Metal dusting of binary Fe-Al alloys in CO-H2-H2O gas mixtures', in Journal of Corrosion Science and Engineering
2003
Zhang J; Schneider A; Inden C, 2003, 'Metal dusting of iron in CO-H2-H2O gas mixtures at 600°C', in Journal of Corrosion Science and Engineering
2003
Zhang J; Ostrovski O, 2000, 'Processing of Iron Ore Using methane-containing Gas,', in International Congress on Mineral Processing and Extractive Metallurgy MINPREX 2000, Melbourne, pp. 509 - 517, presented at International Congress on Mineral Processing and Extractive Metallurgy 2000, Melbourne, 11 September 2000 - 13 September 2000
2000
Zhang G; Ostrovski O; Suzuki K, 2000, 'Iron Ore Reduction and Iron Carburisation by H2-CH4-Ar Gas Mixtures,', in Belton Memorial Symposium, IRON & STEEL SOCIETY, Sydney, pp. 431 - 443, presented at Belton Memorial Symposium, Sydney, 10 January 2000 - 11 January 2000, http://gateway.webofknowledge.com/gateway/Gateway.cgi?GWVersion=2&SrcApp=PARTNER_APP&SrcAuth=LinksAMR&KeyUT=WOS:000169876900034&DestLinkType=FullRecord&DestApp=ALL_WOS&UsrCustomerID=891bb5ab6ba270e68a
2000
Zhang JQ; Wu BY; Wu XH; Wang GQ; Zhao JW, 1995, 'Crystallization behavior of a mechanically alloyed amorphous Fe80Zr8B11Cu1 alloy', in JOURNAL OF APPLIED PHYSICS, AMER INST PHYSICS, PHILADELPHIA, PA, pp. 5473 - 5475, presented at 40th Annual Conference on Magnetism and Magnetic Materials, PHILADELPHIA, PA, 06 November 1995 - 09 November 1995, http://dx.doi.org/10.1063/1.362279
1995
Conference Abstracts
add
Xie Y; Zhang J; Young D, 2018, 'Effect of Fe on corrosion of Ni-20Cr and Ni-30Cr alloys in wet CO2 gas at 650oC', in ISHOC 2018, The Iron and Steel Institute of Japan, Matsue, Japan, pp. 12 - 15, presented at International Symposium on High-temperature Oxidation and Corrosion 2018, Matsue, Japan, 21 October 2018 - 26 October 2018
2018
Yang J; Zhang J; Ostrovski O; Zhang C; Cai D, 2018, 'Effects of B2O3 on cyrstallisation behaviour, structure, and heat transfer of CaO-Al2O3-based mould fluxes', in The 7th Australia-China-Japan Joint Symposium on Iron and Steelmaking, The 7th Australia-China-Japan Joint Symposium on Iron and Steelmaking, Suzhou, China, pp. 35 - 35, presented at The 7th Australian-China-Japan Joint Symposium on Iron and Steelmaking, Suzhou, China, 04 September 2018 - 07 September 2018
2018
Book Chapters
add
Yang J; Zhang J; Sasaki Y; Ostrovski O; Zhang C; Cai D; Kashiwaya Y, 2016, 'Effect of Na2O on Crystallisation Behaviour and Heat Transfer of Fluorine-Free Mould Fluxes', in Advances in Molten Slags, Fluxes, and Salts, John Wiley & Sons, Inc., pp. 335 - 342, http://dx.doi.org/10.1002/9781119333197.ch36
2016
Young DJ; Zhang J, 2008, 'Alloy with copper to reduce metal dusting rates', in Schutze M (ed.), Novel approaches to improving high temperature corrosion resistance, edn. 47, Woodhead Publishing Limied, Cambridge, England, pp. 19 - 35, http://dx.doi.org/10.1533/9781845694470.1.19
2008
Schneider A; Zhang J; Inden G, 2007, 'Metal dusting of ferritic Fe-Al-M-C (M=Ti,V,Nb,Ta) alloys in CO-H2-H2O gas mixtures at 650°C', in Grabke HJ; Schutze M (ed.), Corrosion by carbon and nitrogen, Woodhead Publishing, Cambridge, UK, pp. 175 - 186, http://dx.doi.org/10.1533/9781845693350.175
2007
Zhang J, 2007, 'Coke formation during metal dusting of iron in CO-H2-H2O gas with high CO content', in Grabke HJ; Schutze M (ed.), Corrosion by carbon and nitrogen, Woodhead Publishing, Cambridge, UK, pp. 199 - 213, http://dx.doi.org/10.1533/9781845693350.199
2007
Zhang J; Schneider A; Inden G, 2007, '11 α-Fe layer formation during metal dusting of iron in CO–H2–H2O gas mixtures', in Corrosion by Carbon and Nitrogen, pp. 187 - 198, http://dx.doi.org/10.1533/9781845693350.187
2007
Zhang J; Schneider A; Inden G, 2007, '12 Coke formation during metal dusting of iron in CO–H2–H2O gas with high CO content', in Corrosion by Carbon and Nitrogen, pp. 199 - 213, http://dx.doi.org/10.1533/9781845693350.199
2007
Zhang J; Schneider A; Inden G, 2007, 'α-Fe layer formation during metal dusting of iron in CO-H2-H2O gas mixtures', in Corrosion by Carbon and Nitrogen: Metal Dusting, Carburisation and Nitridation, pp. 187 - 198, http://dx.doi.org/10.1533/9781845693350.187
2007
Schneider A; Zhang J, 2007, '10 Metal dusting of ferritic Fe–Al–M–C (M = Ti, V, Nb, Ta) alloys in CO–H2–H2O gas mixtures at 650°C', in Corrosion by Carbon and Nitrogen, pp. 175 - 186, http://dx.doi.org/10.1533/9781845693350.175
2007
Zhang J; Schneider A; Inden G, 2007, '¡§ƒÑ-Fe layer formation during metal dusting of iron in CO-H2-H2O gas mixtures', in Grabke HJ; Schutze M (ed.), Corrosion by carbon and nitrogen, edn. Original, Woodhead Publishing, Cambridge, UK, pp. 187 - 198
2007
  • Australian Research Fellowship (ARF) 2006 - 2010
  • Max-Planck-Society Fellowship 2002

Research Grants

  • ARC Discovery Grants
    • DP200101612 (2020-2023), $556,200 (Lead CI): High temperature corrosion induced by multiple secondary oxidants
    • DP190101574 (2019-2022), $480,000 (Lead CI): Combined effects of deposits and environmental oxidants on materials degradation in advanced power generation – mechanism and prevention
    • DP150100669 (2015-2018), $399,500 (Lead CI): Controlling nickel-base alloy high temperature corrosion in CO2-rich gases
    • DP130100526 (2013-2015), $460,000 (CI): Heat-resisting iron-nickel base alloys in challenging new applications: oxygen permeabilities and resistance to internal oxidation
    • DP120101243 (2012-2014), $425,000 (Lead CI): Role of oxide grain boundaries in controlling high temperature corrosion of steels by CO2-rich gases
    • DP0880124 (2008-2010), $260,000 (CI): Controlling corrosion of steel by CO2-rich gases at high temperatures
    • DP0665786 (2006-2010), $695,000 (ARF): “Metal dusting” of austenitic alloys: mechanisms and interventions
  • Linkage Projects
    • LP150100591 (2015-2018), $377,000 (CI): Understanding the role of nanoparticles in water based lubrication
    • LP130100773 (2013-2016), $250,000 (CI): Decrease of environmental impact of steelmaking: development of fluorine-free mould flux for steel continuous casting
  • ARC HUB Grant
    • Baosteel project (2017-2020) $150,000 (Lead CI): Development of CaO-Al2O3-based mould fluxes for the continuous casting of high Al steel
  • Baosteel-Australia Joint Centre (BAJC) R&D Projects
    • BA16006 (2017-2020), $150,000 (Lead CI): Investigation of CaO-Al2O3-based mould fluxes for the continuous casting of high Al steel
    • BA12011 (2013-2016), $200,000 (CI): Fluorine-free mould flux for continuous casting

High temperature corrosion of metal materials, and high temperature materials development

  • Phase Transformation
  • Secondary Processing of Metals
  • Process Metallurgy, Advanced
  • Mechanical Properties of Materials
  • Sustainable Materials Processing